O-Ring Supply Co.
ISO Certified
10,000+ O-Ring Sizes
Custom Manufacturing

Carbon Tetrachloride Resistant O-Rings

Compatibility ratings for 7 O-ring materials in Carbon Tetrachloride service

At a glance:A× 3B× 0C× 0D× 43 of 7 materials recommended for Carbon Tetrachloride

Carbon Tetrachloride (Solvents) compatibility with the seven most common O-ring elastomers, rated on the standard A/B/C/D scale: A = excellent, B = good, C = fair, D = not recommended. This data also appears in our interactive chemical compatibility chart and is available machine-readable at /api/chemicals.json.

MaterialRatingGuidance
NBRDnot recommended — rapid degradation expected
FKMAexcellent — recommended for continuous service
EPDMDnot recommended — rapid degradation expected
VMQDnot recommended — rapid degradation expected
PTFEAexcellent — recommended for continuous service
FFKMAexcellent — recommended for continuous service
HNBRDnot recommended — rapid degradation expected

Why These Ratings

  • NBR (D) — documented weaknesses include “Chlorinated hydrocarbons.”
  • FKM (A) — documented strengths include “Chlorinated hydrocarbons.”
  • EPDM (D) — documented weaknesses include “Chlorinated solvents.”
  • VMQ (D) — documented weaknesses include “Chlorinated solvents.”
  • PTFE (A) — documented strengths include “Aromatic and chlorinated solvents.”
  • FFKM (A) — documented strengths include “Aromatic and chlorinated solvents.”
  • HNBR (D) — documented weaknesses include “Chlorinated hydrocarbons.”

SolventsService: Concentration & Temperature Notes

Match solvent polarity to polymer polarity. Ketones and esters (polar) destroy NBR and FKM but suit EPDM; aromatic and chlorinated solvents (non-polar) do the reverse. Aliphatic hydrocarbons such as hexane and heptane are the mildest — NBR rates B to A. Solvent swell is largely concentration-independent, but temperature accelerates both fluid uptake and plasticizer extraction.

Use With Caution

No conditional materials for this chemical.

Avoid

  • NBR (D)
  • EPDM (D)
  • VMQ (D)
  • HNBR (D)
Engineering note: ratings are general guidelines based on typical exposure conditions. Fluid concentration, temperature, pressure and exposure time can shift compatibility by a full grade or more. For critical service, validate the actual compound with ASTM D471 immersion testing before production use. Selecting across multiple chemicals? See the chemical-resistant O-ring selection guide for a material-first comparison.

Frequently Asked Questions

Is Carbon Tetrachloride compatible with FKM (Viton) O-rings?

FKM is rated A for Carbon Tetrachloride: excellent — recommended for continuous service. Ratings are general guidelines; concentration, temperature and exposure time all affect real-world compatibility, so validate critical applications with ASTM D471 immersion testing.

Is Carbon Tetrachloride compatible with NBR (nitrile) O-rings?

NBR is rated D for Carbon Tetrachloride: not recommended — rapid degradation expected. NBR is the lowest-cost elastomer, so when it earns an A or B rating it is usually the economical default; when it rates C or D, do not substitute it for a higher-rated material to save cost.

Can I use PTFE O-rings with Carbon Tetrachloride?

PTFE is rated A for Carbon Tetrachloride: excellent — recommended for continuous service. Remember that PTFE has no elastic memory — in demanding service it needs spring energization or an elastomer core (FEP/PFA encapsulation) to maintain sealing force.

What is the best O-ring material for Carbon Tetrachloride?

FKM, PTFE, FFKM are rated A (excellent) for Carbon Tetrachloride in our compatibility data and are the recommended starting point for material selection. Final selection should also account for operating temperature, pressure and whether the seal is static or dynamic.

Can I use EPDM O-rings with Carbon Tetrachloride?

EPDM is rated D for Carbon Tetrachloride: not recommended — rapid degradation expected. Always confirm the specific fluid concentration and temperature before specifying EPDM for this service.

Need O-Rings for Carbon Tetrachloride Service?

Send us your fluid, concentration and temperature — our engineers will confirm the right compound. MOQ 1 piece.